Zinc Telluride
ZnTe

Crystal properties

Crystal growth method

Seeded Vapor-Phase Free Growth Technology

Crystal growth orientation

(100) (110) (111) +/- 0.5°

Crystal structure

cubic, a = 6.1034Å

Growth direction

<111>

Specific resistivity

< 1 X 106 Ohm cm

Hall mobility

130 (h) cm/ V / sec.

EPD

< 5 X 105 / cm2

Twin

Twin free

Orientation

Size

Polish

(100)

10*10*1mm3

Both sides

(110)

10*10*1mm3

Both sides

(111)

10*10*1mm3

Both sides